Requested by Hagitec co., ltd.
Test: Commpression breaking load test
Product: Fiber Protector Pipe length:100m
Material:SUS304
Date:08/28/1986
Results: As of the table below.
|
Chibaken Mechanical-Metal Examination Institute
Manager: Miyata
| Type |
Compression weight at the breaking point |
Test Method |
| KS-5N |
540Kgf |
 |
| KS-1.8N |
600 |
| SA-4N |
830 |
| IS-4N |
1100 |
| KS-7N |
340 |
| SX-8N |
1150 |
| SASP-8.5N |
760 |
|
|
Requested by Hagitec co., ltd.
Test:Tensile Strength Test
Product: Fiber Protector Pipe length 200m
Material:SUS304
Date:08/28/1986
Results: As of the table below.
|
Chibaken Mechanical-Metal Examination Institute
Manager: Miyata
| Type |
maximum tensile weight |
| KS-5N |
23kgf |
| KS-1.8N |
20 |
| SA-4N |
23 |
| IS-4N |
60 |
| KS-7N |
106 |
| SX-8N |
224 |
| SASP-8.5N |
124 |
|
|